Both of these should work pretty well on AKA 870s.
Infil density: 10% is good enough ( Please note that since the walls aren't thick in the first place, 10% basically equals 100%....you will see )
DON'T use brims. Brims can cause failure to eject, just use skirt or nothing.
870_shell_5.stl:
- Much more durable.
- More printing time
- Decent muzzle velocity
- I suggest using this one if you are not in a rush.
870_shell_4.stl:
- Less durable
- Less printing time (probably only decreases by about 15 mikes / shell)
- I suggest using this one if you need a huge amount of ammo in a short time (e.g. wargame tmr)